COATINGS


Metal Matrix Composite

KM enables the low cost preparation of PRMMC materials and coatings. Several examples of metallic and ceramic reinforcements are illustrated in the micrographs below
  • Reinforcement up to 70 V %
  • Strength enhancement up to 100%
  • Part density up to 100%
  • High specific strength and stiffness
  • Up to 200% of matrix material


Al-Al203 350X
Al-SiC 350X
Al-Ti 400X
Al-Fe 400X
Al-Ni 400X


Contact Us   |     Literature   |    KM Conferences  |     Careers   |     Site Map